TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
Chris Gardini-ECG005 <[log in to unmask]>
Date:
Fri, 22 Aug 1997 13:24:49 -0500
X-cc:
"Jim Drass-EJD001 (Receipt Notification Requested)" <[log in to unmask]>
Comments:
( Received on motgate.mot.com from client mothost.mot.com, sender [log in to unmask] )
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Chris Gardini-ECG005 <[log in to unmask]>
Parts/Attachments:
text/plain (10 lines)
Seeking data/reports to address questions on the risks associated with
Annular Ring size.  In particular, as the mis-registration of the of the
mechanical drill to the PTH Pad moves towards a trace leading into the pad
the potential for an 'open' to occur increases.  Concerns center around
'thin' ring passing ET, but in field stresses cause fracture and crack
propagation to 'open' state.

Thanks, Chris