TECHNET Archives

December 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 5 Dec 2007 10:56:44 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (236 lines)
Especially since the material will be setting up on its own.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Wednesday, December 05, 2007 10:29 AM
To: [log in to unmask]
Subject: Re: [TN] Solithane 113/C113-300 conformal coating (Dipping)

GA Tan
I would ask as well why you want to use this material.  It was
originally 
developed for high voltage space applications, but NASA found some 
problems with the material.  You might want to read this NASA Technical 
Brief before spending a lot of time setting up for this material.

http://code541.gsfc.nasa.gov/documents/materials_tips_PDFs/TIP%20011R.pd
f

Doug Pauls
Rockwell Collins




Graham Naisbitt <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
12/05/2007 09:38 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Graham Naisbitt <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Solithane 113/C113-300 conformal coating (Dipping)






GA Tan

To my knowledge this coating was developed for space programmes 
because it features low or no out-gassing.

The material is quite tricky to handle and apply correctly and, again 
if my memory is not deserting me, it is 2 component. This means that 
it is really undesirable for dipping because you will throw away far 
more than you will use.

If you send me a copy of the data sheet, I can probably give more 
advice.

Kindest regards
Graham Naisbitt

[log in to unmask]

www.gen3systems.com

Phone: +44 (0)12 5252 1500
Mobile: +44 (0) 79 6858 2121


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------

Gen3 Systems Limited
Unit B2, Armstrong Mall
Southwood Business Park
Farnborough Hampshire
GU14 0NR - UK

ENGINEERING RELIABILITY
IN ELECTRONICS

Registered Number: 4639449 (England & Wales). Registered Office as 
above.
DISCLAIMER : This message is intended only for the use of the 
individual or entity to which it is addressed and may contain 
information which is privileged, confidential, proprietary, or exempt 
from disclosure under applicable law. If you are not the intended 
recipient or the person responsible for delivering the message to the 
intended recipient, you are strictly prohibited from disclosing, 
distributing, copying, or in any way using this message. If you have 
received this communication in error, please notify the sender and 
destroy and delete any copies you may have received. Any views or 
opinions presented in this email are solely those of the author and 
might not represent those of Gen3 Systems Limited. Although Gen3 
Systems Limited has taken reasonable precautions to ensure no viruses 
present in this email, Gen3 Systems Limited can not accept the 
responsibility for any loss or damage arising from the use of this 
email or attachments.




On 5 Dec 2007, at 09:10, Tan Geok Ang wrote:

> Hi All,
>
>             I need help and guidance on dipping conformal coating 
> of Solithane.
>
>             Can anyone provide me with some guidance on "Dipping 
> and Rework" processes and requirement (not spray).
>
>                 a) What is the right viscosity of the mixture 
> between Solithane 113 and C113-300? To ensure right coating and to 
> eliminate bubbles effects?
>
>                 b) What temperature to set to ensure the process 
> (thickness) consistence during the dipping process
>
>                 c) Must there be another air spray (temperature 
> control?) process  to ensure the coating thickness.
>
>                 d) What is the speed on dipping and removing?
>
>
>
>                 e) What will be pot life of the mixture?
>
>                 f) What is the recommended curing method 
> (temperature curve? or must be 5days or 10days requirement)
>
>                 g) If there are connectors, other then using RTV to 
> cover these connector. Is there any other better and consistent 
> matter to ensure that coating mixture does not move into the 
> connectors?
>
>                 h) What chemicals is/are available to remove/rework 
> on the coating if a component needs to be replaced? What other 
> things must be taken note of?
>
>                 i) If the PCBA is cleared, should I bake those PCBA 
> before the process (or same temperature as the coating mixture just 
> before use?)
>
>
>
> Sorry that I have some many questions as I am task to work and 
> develop on this process and implement it within a month so your 
> help and guidance is greatly appreciated! Thanks
>
>
>
> Best Regards
>
> GA Tan
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following 
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail 
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/ 
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp? 
> Pageid=4.3.16 for additional information, or contact Keach Sasamori 
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2