http://www.astm.org/Standards/B571.htmhttp://www.ipc.org/ContentPage.aspx?PageID=4.1.0.1.1.4
Hi Linda,
No this is an ASTM procedure (see link). IPC does have adhesion tests in TM-650. Check out 2.4.1 (see IPC link)
Best regards,
Dave
David W. Bergman 大山人
Vice President, International Relations
IPC - Association Connecting Electronics Industries
3000 Lakeside Drive Suite 309 S Bannockburn, IL 60015-1249 USA
+1 847-597-2840 tel
+1 847-615-5640 fax
+1 847-867-1388 mobile
[log in to unmask]
www.ipc.org
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Linda Langley
Sent: Wednesday, April 08, 2009 9:23 AM
To: [log in to unmask]
Subject: [TN] Plating over metal
Is ASTM B571 an IPC document? Any one know where I could find a copy?
It is supposed to be a standard for plating over metal.
Linda Langley CIT
Training Specialist
Jabil Circuit
248-292-6176
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------