[log in to unmask] wrote:
>
> Hi everyone!
>
> I would be appreciative of any help whatsoever on the following
> subject:
>
> I am currently assessing the suitability of using no-clean flux
> technology on Class 3 Electronics - Military. Our current capability
> is double sided Reflow (forced convection), Vapour Phase & Wavesolder.
> We assemble onto the following substrates - FR4, Copper Invar Copper,
> Ceramic. SMD design is currently @ 0.02" pitch, whilst currently
> evaluating 0.016" & BGA.
>
> I am trying to identify all areas of concern with using no-clean flux
> to enable me to come up with a plan for addressing/proving the process
> for suitability/reliability. I believe I have identified the main
> areas but would be interested in the experience/views of my
> counterparts in this field.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
If you are going conformal coat the PWBs then this will be a concern.
The boards MUST be cleaned if conformal coating is to be used.
Regards,
Brent
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|