TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Stephen Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 14 Mar 2005 10:28:06 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (137 lines)
Thornton,

I wouldn't load a BGA without solder paste on to a ENIG finished
PCB. Even though the gold is probably pretty thin, without the additional
solder from the paste, you're taking a chance of gold embrittlement.

I know that there are those that say one only needs flux for BGA rework
if the BGA has eutectic spheres, but I feel that the extra volume of solder
from the paste gives the BGA more stand-off, thus more reliable.

As for a mini-stencil a US company called Circuit Technology Center
makes something called "Flextac Stencils". I've used them on numerous
occasions, the most recent was when I had to rework a 676-ball, 1mm pitch
Xilinx BGA.

The Flextac stencils can be obtained from:

Intertronics
Unit 17, Station Field Industrial Estate
Banbury Road
Kidlington
Oxfordshire
OX5 1JD
England

+44 (0) 1865 842842 Phone
+44 (0) 1865 842172 FAX

Here's a link to Intertronics web site about them:

http://www.intertronics.co.uk/products/flextac.htm

Here's another link to all the BGA patterns available as the Intertronics
wb page didn't seem to show all the different pattuerns that are available.

http://www.circuittechctr.com/products/201-3120s.shtml

Another product that is fairly new on the market for BGA rework is
something
called "StencilQuik". It's basically a polyimide, or kapton, stencil that
is placed
over the BGA footprint, paste stenciled into the apertures, the BGA placed
(can
literally be done by hand), and then the BGA reflowed. The StencilQuik
stencil
then becomes a permanent part of the assembly.

I have no direct experience with StencilQuik, but it does seem rather
interesting.
Here's a link to it:

http://solder.net/stencilquik/default.asp

Kind regards,

-Steve Gregory-



|---------+---------------------------->
|         |           Thornton White   |
|         |           <thornton.white@C|
|         |           EMTRON.COM>      |
|         |           Sent by: TechNet |
|         |           <[log in to unmask]>|
|         |                            |
|         |                            |
|         |           03/14/2005 09:25 |
|         |           AM               |
|         |           Please respond to|
|         |           TechNet E-Mail   |
|         |           Forum; Please    |
|         |           respond to       |
|         |           Thornton White   |
|         |                            |
|---------+---------------------------->
  >--------------------------------------------------------------------------------------------------------------|
  |                                                                                                              |
  |       To:       [log in to unmask]                                                                              |
  |       cc:                                                                                                    |
  |       Subject:  [TN]                                                                                         |
  >--------------------------------------------------------------------------------------------------------------|




Hi All.

We have a customer who wants us to place BGA's for them on otherwise
comletely loaded PCB's.
Problem is, the BGA apertures were missed from their stencil.

Is it at all possible to load a BGA straight on to an unpasted (gold
finish)
card? What are the quality implications?
Assuming the answer to above is NO, does anyone have UK contacts for BGA
mini-stencils

Any advice would be appreciated.

Thanks in advance.
Thornton

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------




__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2