TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Kane, Amol (349)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Kane, Amol (349)
Date:
Fri, 29 May 2009 16:21:09 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (206 lines)
Certainly does, thanks again and have a nice weekend!

-----Original Message-----
From: Graham Naisbitt [mailto:[log in to unmask]] 
Sent: Friday, May 29, 2009 11:34 AM
To: Kane, Amol (349)
Cc: TechNet E-Mail Forum
Subject: Re: [TN] Humiseal 2A64 CC Experiences

Amol

Under most circumstances I would recommend dipping as you can better  
guarantee to get the coating under, as well as over, the components.

Whether you dip, spray or thrown it on from a bucket don't matter a  
darn, as long as the finished product passes your tests. The issue is  
purely one of proper coverage to get the most performance out of the  
coating.

Spraying can give you what you need, but it requires more effort to  
seal off the underside or get it behind the component legs. There are  
ways and means to do that, and you can download my Conformal Coating  
Facts & Data Handbook from my web site that might help you further.

If your customer insists on dipping, then make sure you build-in  
enough cost to cover for the wastage that will be huge. And don't  
forget to add for a lot of stripping solvent to clean-up between mixes.

I know many customers who spray coat and pass salt fog tests. Salt  
mist and salt spray might be another matter. To get the best  
protection and keep the process under reasonable cost control, then  
use a 1 part coating.

Trust this clarifies my point?

Regards

Graham Naisbitt

Email: [log in to unmask]
Phone: +44 (0)12 5252 1500
Web: www.gen3systems.com

On 29 May 2009, at 15:34, Kane, Amol (349) wrote:

> Thank you very much Graham for your insights!....can you touch on  
> the issue of whether dip coating is better suited to resist a salt  
> fog environment as compared to spray coating? With all other  
> parameters being the same, the only difference I can see is that dip  
> coating method has more exhaustive coverage on the PCB as it can  
> cover under components, which the spray coating method cannot.
>
> Thanks again,
> Amol
>
>
>
> -----Original Message-----
> From: Graham Naisbitt [mailto:[log in to unmask]]
> Sent: Friday, May 29, 2009 10:11 AM
> To: TechNet E-Mail Forum; Kane, Amol (349)
> Subject: Re: [TN] Humiseal 2A64 CC Experiences
>
> Hi Amol
>
> Do NOT attempt to dip coat with 2A64, unless you are happy to throw
> away the majority of it after around 4 to 6 hours.
>
> This is a 2 part urethane, and 1 part is moisture sensitive.
>
> Spray coating is your best option by far. If quantities to coat are
> few, then mix and spray as desired but the pot life when mixed is only
> a couple of hours before rheology and viscosity drift too far.
>
> If quantities are high, then I suggest having each part mixed via a
> pump system complete with spiral mixer. This way you minimise wastage
> but the spiral mixer and pump circuit need thoro purging.
>
> You might keep in mind that 1A20 was designed to replace 2A64 as a one
> part material with similar performance characteristics.
>
> If I was you, I would stick with 1A33 - it will do all you want but if
> its not on the drawing, then 2A64 it will be.
>
> Regards
>
> Graham Naisbitt
>
> Email: [log in to unmask]
> Phone: +44 (0)12 5252 1500
> Web: www.gen3systems.com
>
> On 29 May 2009, at 13:34, Kane, Amol (349) wrote:
>
>> Dear Technet Gurus,
>> I am looking for any experiences you may have with the 2A64 coating.
>> We currently spray other urethanes (1A33, 1A20 etc), but not have
>> had any experience with this particular coating. Looking for info on
>> whether this is used in spray or dip application (the TDS says it
>> can be used in either, but is there a particular method it better
>> lends itself to?), any peculiar characteristics that other urethanes
>> from Humiseal do not have, general experience working with this
>> material.
>>
>> Also, which application method (spray vs. dip) is better to resist a
>> salt spray/salt fog environment? You can reply offline if you so
>> choose.
>>
>> Thanks in advance,
>> Amol
>>
>>
>>
>> WARNING:  Export Control
>> This document may contain technical data within the definition of the
>> International Traffic in Arms Regulations (ITAR), and subject to the
>> Export
>> Control Laws of the U.S. Government.  Transfer of such data by any
>> means to a
>> foreign person, whether in the United States or abroad, without
>> proper export
>> authorization or other approval from the U.S. Department of State is
>> prohibited.
>>
>> CONFIDENTIALITY NOTICE:
>> This e-mail, and any attachments, is for the sole use of the intended
>> recipient(s) and may contain information that is confidential and
>> protected from disclosure under the law. Any unauthorized review,  
>> use,
>> disclosure, or distribution is prohibited. If you are not the  
>> intended
>> recipient, please contact the sender by reply e-mail, and delete/
>> destroy
>> all copies of the original message and attachments.
>> Thank you.
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following
>> text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail  
>> to [log in to unmask]
>> : SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]
>> : SET Technet Digest
>> Search the archives of previous posts at: http://listserv.ipc.org/archives
>> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at [log in to unmask]
>> or 847-615-7100 ext.2815
>> -----------------------------------------------------
>
>
>
>
> WARNING:  Export Control
> This document may contain technical data within the definition of the
> International Traffic in Arms Regulations (ITAR), and subject to the  
> Export
> Control Laws of the U.S. Government.  Transfer of such data by any  
> means to a
> foreign person, whether in the United States or abroad, without  
> proper export
> authorization or other approval from the U.S. Department of State is
> prohibited.
>
> CONFIDENTIALITY NOTICE:
> This e-mail, and any attachments, is for the sole use of the intended
> recipient(s) and may contain information that is confidential and
> protected from disclosure under the law. Any unauthorized review, use,
> disclosure, or distribution is prohibited. If you are not the intended
> recipient, please contact the sender by reply e-mail, and delete/ 
> destroy
> all copies of the original message and attachments.
> Thank you.




WARNING:  Export Control 
This document may contain technical data within the definition of the 
International Traffic in Arms Regulations (ITAR), and subject to the Export 
Control Laws of the U.S. Government.  Transfer of such data by any means to a 
foreign person, whether in the United States or abroad, without proper export 
authorization or other approval from the U.S. Department of State is 
prohibited. 
 
CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy 
all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2