Steve,

Thanks! It makes communication simpler.

David A. Douthit
Manager
LoCan LLC

Steve Gregory wrote:

>Hi Dave!
>
>I've put your paper up on my page. Go to: http://www.stevezeva.homestead.com
>and look for "DavesPaper.pdf"
>
>-Steve Gregory-
>
>P.S. Be patient after you click on it, it's a 945 KB file...takes a bit to
>download.
>
>
>
>
>>Hi Gang! I'll take a swipe at finding the middle ground on this one! Both
>>Graham and Dave are correct from each of their perspectives - Graham has a
>>multitude of real life use data of AR type conformal coating being used in
>>a number of severe use environments successfully and Dave has been involved
>>in some of the "uglier" aspects of when AR type conformal coating is an
>>incorrect application for a given use environment. Collins published a
>>paper on an investigation comparing AR and Paralyene conformal coating
>>types with BGA style components. The investigation shows both coating types
>>work well and the application method (as other TechNetees have mentioned)
>>can be critical in impacting solder joint reliability. Steve - if I send a
>>copy of the paper can you put it out on your website?
>>
>>Dave Hillman
>>Rockwell Collins
>>[log in to unmask]
>>
>>
>>
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
>
>
>


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2