Regarding the CTE value for aramid fiber, it is most often listed as -2 ppm/C
in the x,y and around 60 ppm for the z-axis.  I should mention that the CTE
value of the reinforcement fiber is often very low when compared to the CTE
values for the resin system that can be a more dominate factor (especially the
z-axis).  The CTE value for copper is 14-16 ppm, 23 ppm for SnPb, so there is
a dog's breakfast of material CTEs to deal with before you make your decision
about the reinforcement material.
Your second question on technical papers and information sources for
controlled expansion materials and designs, I would suggest that you give Joe
Leibowitz at Shirline Composites a call.  He can be reached at 310-558-4888.
Joe has done work with carbon fiber as well as mixtures of aramid fiber,
carbon and quartz and has published and given several IPC technical papers on
this subject.

Regards,
Lyle Wallig

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2