Look again at Table 3.2, under code C.
Under section C where it says Minimum Wrap (right below Copper - minimum
average, and Minimum thinc areas). For class 3 the minimum wrap would be
.472 mils thickness extending from the hole edge outward .984 mils.
Not sure where you are getting overhang from?
Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Seymour
Sent: Thursday, January 24, 2008 3:28 PM
To: [log in to unmask]
Subject: [TN] ipc-6012B amendement
Howdy,
Section 3.6.2.11.1 of the 6012 amendment Dec 2006 talks about
the Minimum Wrap on a via filled hole.
In Diagram 3-13 there is a measurement labeled "Minimum Copper Thickness",
which is shown as the thickness of the Wrap.
Where is the table that shows the "Minimum Copper Thickness" by Class?
Table 3-2 only talks about the amount of the overhang of the wrap, not the
thickness as such. Table 3-2 has something called Min Thin areas, but this
is not labeled in the diagram 3-13.
Am I missing something?
Thanks
Dave
--
Dave Seymour, CID+
Catapult Communications Inc.
800 Perimeter Park Dr, Suite A
Morrisville, NC 27560
Direct: (919)653-4249
Main: (919)653-4180
Fax: (919)653-4297
[log in to unmask]
****************************************************************************
*****************************
"This e-mail (and any attachments) is confidential and privileged
information of Catapult Communications"
****************************************************************************
*****************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|