Subject: | |
From: | |
Date: | 09 Dec 96 10:03:24 -0500 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
All soldermasks lose adhesion after a wave profile. If you have a 20%
loss, check all processes for loss of temperature control. It could
also be a supplier issue with dirty panels prior to mask application.
______________________________ Reply Separator _________________________________
Subject: Soldermask peeling
Author: [log in to unmask] at internet
Date: 12/9/96 8:36 AM
We recently experienced soldermask peeling after wave from
three different Fabricators all within 2 weeks. Subsequently
we took sample lots of each Fabricator and performed a
pre-wave and post-wave tape test. In all lots the boards
passed pre-wave tape test but had a 10-25% failure post wave.
What can cause this phenomena? Does the weather change have
anything to do with soldermask application and durability?
Dan Hickey
Senior Buyer
Vicor
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|