Wrong. There will be no whiskers after it has gone through the wave.
Bogert wrote:
>
> Wrong. Pure tin will grow tin whiskers.
> ----- Original Message -----
> From: "Brian Ellis" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Thursday, October 25, 2001 3:36 AM
> Subject: Re: [TN] Adjusting the alloy composition in the solderpot
>
> > Here's an interesting thought:
> >
> > If we ask all the component manufacturers (incl. bare boards) to use
> > pure tin for their lead coatings etc., instead of tin/lead, this would
> > a) satisfy the lead-free guys
> > b) help keep the proportions right in the solder pot
> >
> > Right?
> >
> > Brian
> >
> > "d. terstegge" wrote:
> > >
> > > Hi Technet,
> > >
> > > I just received an analyses report for our solder bath composition, and
> my Sn level is at 61.5 percent instead of the nominal 63 percent. This is at
> the edge of the J-STD-001C specification, so I'll have to add some pure tin
> to the pot.
> > > Last time was many years ago, and unfortunately I forgot the formula for
> calculating the amount of tin to add.
> > > It can't be that difficult, but I thought it would be quicker to ask.
> > >
> > > Thanks,
> > >
> > > Daan Terstegge
> > > SMT Centre
> > > Thales Communications
> > > Unclassified mail
> > > Personal Website: http://www.smtinfo.net
> > >
> >
> > --------------------------------------------------------------------------
> -------
> > > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> > > To unsubscribe, send a message to [log in to unmask] with following text
> in
> > > the BODY (NOT the subject field): SIGNOFF Technet
> > > To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> > > Search previous postings at: www.ipc.org > On-Line Resources & Databases
> > E-mail Archives
> > > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> > > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> >
> > --------------------------------------------------------------------------
> -------
> >
> > --------------------------------------------------------------------------
> -------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> > Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> > --------------------------------------------------------------------------
> -------
> >
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|