Bob,
My feeling is mixed on interposers in use with BGAs, I like interposer on flat preferably gold lands hence how do you use that with a BGA.... For me re-balling is required as the leaded assembly reflow temp profile is not high enough to properly reflow your no-lead balls. I like leaded assembly, I like unleaded assembly, I like matte tin finish leads in leaded and unleaded assembly however the BGA ball is not a finish -it is a volume of material- and it's engineered collapse must be how it was intended.
Rough reflow numbers 215 for leaded and 260 for unleaded.
One point is that matte tin in a leaded assembly wants to have 100% coverage of the matte tin finish; the concern in long life apps being the whisker. The BGA refloat is not a whisker issue... although I don't want to start chasing my tail here...
Boston Brad
----- Original Message -----
From: Bob Landman<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Friday, July 09, 2010 10:05 AM
Subject: [TN] Interposer for SAC BGA
I have to use a new FPGA from Lattice and they are not offering it in SnPb, only SAC balls. This is a fpBGA 23mm sq with 484 balls in a square array with no special heatsink pads.
Environment is -40 to +85C, mild vibration and shock, outside environment in electrical NEMA enclosures.
SnPb is a must - I refuse to use lead free process for our products.
Two choices:
Interposer board (Bill Rollins just told me about this option
Reballing
Comments please on your preference.
Bob Landman
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|