Howard-
I don't think NELCO has a web site, though you may want to look at
http://www.parkelectro.com/ar98/, on Park Electrochemical's site (NELCO
is a subsidiary of Park Electrochemical). They are a major supplier of
BT epoxy laminates and prepregs.
You may also want to call NELCO Phoenix ofice at 602-967-5600.
M. Alderete
YOU WROTE....
------------------------------
Date: Thu, 16 Jul 1998 00:38:14 +0800
From: Howard Lin <[log in to unmask]>
Subject: Re: Nelco web site
Who can tell me the Web site of Nelco C.C.L company?
Thanks for your help,
Regards
------------------------------
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|