TECHNET Archives

May 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Hinners Hans M Civ WRALC/LUGE <[log in to unmask]>
Date:
Thu, 13 May 2004 20:18:28 -0000
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Hinners Hans M Civ WRALC/LUGE <[log in to unmask]>
Parts/Attachments:
text/plain (50 lines)
Victor,

Postlam bake can reduce or eliminate warp permanently, if it is done right.
We didn't have a choice when the warp was due to unbalanced constructions
(impedance jobs).  If the cause was process related then it was permitted
but not desired.

Hans
Electronics Engineer
WR-ALC
Robins AFB, GA

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez
Sent: Wednesday, May 05, 2004 1:09 PM
To: [log in to unmask]
Subject: [TN] Raw Card warpage

Fellow TechNetters,

   At a PWB factory setting is a final baking process permissible to
correct any warpage prior to customer shipment.   Once the sealed bag is
open and product not used for an extended period of time will the warpage
return.

Victor G. Hernandez

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2