TECHNET Archives

February 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Genny Gibbard <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Genny Gibbard <[log in to unmask]>
Date:
Wed, 6 Feb 2008 14:43:13 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (21 lines)
So,...
During assembly, say that you see SAC solder wicking up the pins of a
finepitch surface mount header onto the contact area which is
gold-plated.  The gold-plated header normally mates with gold socket
connector.  
What would be the reliability issues with SAC solder in contact with the
gold socket?  Does the silver in the solder mitigate any of the
tin-to-gold issues I have been reading about?

Genny

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2