Good morning everyone,

We are seeing a film on some circuit board assemblies after
a pass through our in-line cleaner.

We are using an RA flux and a soaponifier in the cleaner.
The film is only showing up on boards that have a high gloss
LPI mask.
Multiple passes through the cleaner will not remove the
film.
The film can be easily wiped off with a dry wipe.
The film can be cleaned off brushing with isopropyl alcohol
The pattern of the film is an image of the flux residue that
was on the board prior to cleaning.

Any ideas as to what is going on.

Thanks in Advance,
Gary Camac

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2