TECHNET Archives

December 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Kristi Howe <[log in to unmask]>
Date:
Fri, 10 Dec 2004 09:10:21 +0800
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, don_well <[log in to unmask]>
Content-type:
text/plain; charset=gb2312
Subject:
From:
don_well <[log in to unmask]>
Content-transfer-encoding:
7BIT
Parts/Attachments:
text/plain (39 lines)
 Kristi
    Could you tell me what kind of solder paste dispensing machine you used.How to deal with tombstone defect.

B.regards
don
----- Original Message -----
From: "Kristi Howe" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, December 09, 2004 1:51 PM
Subject: Re: [TN] 0201mil chip (0603mm) hot air rework method


> Hello all,
> We use an Edsyn Hot air pencil and solder paste dispensing gun as to not
> add excessive solder with wire.  The pencil is set on 650F and the air flow
> is turned almost all the way off.
> Hope this helps.
> Kristi
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2