TECHNET Archives

December 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Fri, 14 Dec 2001 12:45:47 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
Organization:
Dynamic & Proto Circuits
From:
Brock Hunter <[log in to unmask]>
Parts/Attachments:
text/plain (111 lines)
Karla,

We have an EIE RP-508 and have only been down once in the past 14 months. Overall we are quite
pleased with it. Initially it was intended to supplement our CSI FIRE 9300 and quickly took
over all the work, typically 130 - 150 plots ( 24 X 30 ) per day.

Cheers,

Brock

Karla Thompson wrote:

> Thanks for the replies.
>  Anyone have an EIE plotter? Specifically the RP200 line?
>
> -----Original Message-----
> From: Mark Hargreaves [mailto:[log in to unmask]]
> Sent: Friday, December 14, 2001 04:28
> To: [log in to unmask]
> Subject: Re: photoplotters
>
> Hi Karla,
> We currently have a 3-4 year old CSI (guess it's Gretag now) plotter. We're
> happy with the images, speed and up-time.
>
> Regards,
> Mark Hargreaves
> EMDS
>
>         -----Original Message-----
>         From:   Karla Thompson [SMTP:[log in to unmask]]
>         Sent:   Thursday, December 13, 2001 6:28 PM
>         To:     [log in to unmask]
>         Subject:        [TN] photoplotters
>
>         I'm in the process of looking at Photoplotters and would appreciate
> any
>         input any of you may have. We currently have a 5-6 year old Barco
> Crescent
>         30.  I'm looking at EIE, Orbotech, and Barco/Mania. If any of you
> have any
>         comments on those, or any others (?) I'd appreciate it.
>
>         Karla Thompson
>         CAM Technician
>         Electronic Controls Design, Inc
>         Tel: (503) 829-9108
>         email: [log in to unmask]
>
> ----------------------------------------------------------------------------
> -----
>         Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8d
>         To unsubscribe, send a message to [log in to unmask] with following
> text in
>         the BODY (NOT the subject field): SIGNOFF Technet
>         To temporarily halt delivery of Technet send the following message:
> SET Technet NOMAIL
>         Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
>         Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
>         information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
>
> ----------------------------------------------------------------------------
> -----
>
> ----------------------------------------------------------------------------
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> ----------------------------------------------------------------------------
> -----
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

--
Brock Hunter  [log in to unmask]
Engineering Mgr.
Dynamic & Proto Circuits
TEL (905) 643-9900
FAX (905) 643-9437
http://www.dapc.com

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2