A customer of mine feedback to me that they discovered the warpage of FR4
laminate have systematic relationship with the thickness variation in a
panel. In another word, my customer is saying that the greater the
variation in the laminate thickness the greater will be the warpage.
Example, a piece of 0.062" thickness warped FR4 laminate which has a
thickness variation of range 0.058 - 0.069"(ie some points are higher than
the other), the warpage is found to be high on thickness that higher than
the other. Is it true?
Can someone tell me does the laminate thickness variation have a systematic
relationship with bare board warpage?
Is the z- expansion CTE different between different thicknesses of the same
type of material?
Joseph
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|