TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 8 Oct 2004 17:17:30 +0200
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Daan Terstegge <[log in to unmask]>
Subject:
MIME-Version:
1.0 (Generated by Clearswift ES version 4.8.1.149)
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
From:
Daan Terstegge <[log in to unmask]>
Parts/Attachments:
text/plain (64 lines)
Hi Tom,

In my interpretation such balls are not process indicators but defects.

The fact that these balls don't become dislodged during washing doesn't
mean that they will keep being adhered to the board when the product is
submitted to shocks or vibrations.  But is depends on the service
condition of the product.



Best regards,

Daan Terstegge
PCB Assembly Department
Thales Land & Joint Systems

Tel        +31(0)35 524 8297
Fax       +31(0)35 524 8181
[log in to unmask]
Unclassified Email

>>> [log in to unmask] 10/08/04 04:35pm >>>
Dear Group,
I'm asking the group again to impart your communal wisdom in
interpreting
IPC-A-610. We are seeing solder balls on our SMT assemblies after they
have
gone thru board wash (dishwasher). Would these be classified as
entrapped/encapsulated and therefore process indicators and not
subject
to "rework" (as long as they don't violate minimum electrical
clearance)?
Thanks.

Tom Moore

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2