All wave solder systems have a backup over temp sensor that automatically shuts off the solder pot.
On the Electrovert the spring loaded RTD is mounted on the rear of the solder pot.
This simple circuit is the fail safe for a short or faulty temperature controller or stuck contactor.
In fact when the spring tension is reduced from the constant high heat, in about 6-7 years, the pot may fail to come on.
I saw a tech chase the problem and change everything before he asked for help and I showed him the over temp sensor that needed another 1/2 turn of the adjustment screw.
The mercury relays have a higher switching speed and are used for tighter process controls.
PS Did you know that all the Plasma flat screen TVs have a mercury coating.
John Goulet
----- Original Message -----
From: "Ed Popielarski" <[log in to unmask]>
To: [log in to unmask]
Sent: Thursday, September 23, 2010 5:15:32 PM
Subject: Re: [TN] Wave Temperature Overshoot
Be advised mercury containing devices may be an issue in your state as
is in mine.
Another warning is solid state relay failure mode is typically in the
"on" condition, which could cause overheating, so a failsafe backup
would be advised (yes, solder CAN boil!).
Regards,
Ed Popielarski
Sr. Mfg. Engr.
NBS Corporation
2950 Patrick Henry Dr.
Santa Clara, Ca. 95054
Ph: 408-654-1100
Fx: 408-654-1107
Cl: 408-234-1497
Cl: 949-581-6601
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Wednesday, September 15, 2010 9:49 AM
To: [log in to unmask]
Subject: Re: [TN] Wave Temperature Overshoot
Rex,
If you have a wave solder that uses contactors you may want to replace
them with wetted Mercury devices or SSRs...
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rex Waygood
Sent: Wednesday, September 15, 2010 9:18 AM
To: [log in to unmask]
Subject: Re: [TN] Wave Temperature Overshoot
Thanks for all the inputs.
I think that the problem is cured but we are waiting a bit longer before
we celebrate!
The main contactor had one set of contacts that were sticky. We
disconnected the set of heaters associated with those contacts and the
bath stabilised correctly. The new contactor is now fitted and we are
keeping an eye on it.
Regards
Rex
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Goulet
Sent: 15 September 2010 16:10
To: [log in to unmask]
Subject: Re: [TN] Wave Temperature Overshoot
The Electrovert wave solder has a boost heater that turns on along with
the standard control heater for when the solder pot is shut down.
In the Electrovert manual you will see that you are supposed to use the
provided thermal blanket to cover the solder pot to prevent solder
eruptions and reduce heat loss. I think if you were to log the current
use, you would find that you aren't reducing cost by allowing the solder
pot to cool off to the solid state and then require two heaters to work
almost maximum duty cycle to bring the pot back up to temperature every
day. The shut down procedure is usually reserved for over the weekend
only.
A better method may be to create a low temp recipe "Daily Shutdown"
where the solder pot temp is reduced to 363F and the thermal blanket is
placed over the pot to further reduce heat loss over the evening and
night time hours. The booster heater would not come on, preventing the
early failure of this heater, the temperature overshoot should not occur
if the thermocouple is clean of dross and where there would be no
shrinkage as Paul Edwards referenced. The PID will have a slower ramp up
speed and prevent the over shoot. The thermal blanket reduces heat loss
and the time to reach the desired pot temperature is greatly reduced and
therefore reduces your cost. You may want to consider this process for
your daily routine.
- As I recall the Vitronics wave allows you to set the temperature as
well as the time for a soft shut down, which we used every day.
John Goulet
Sr. Process Engineer
----- Original Message -----
From: "Paul Edwards" <[log in to unmask]>
To: [log in to unmask]
Sent: Thursday, September 2, 2010 12:29:51 PM
Subject: Re: [TN] Wave Temperature Overshoot
The temperature overshoot is can be caused by and in many cases is
caused by the change of the phase of the solder between the heaters and
the thermal sensor...As solder cools shrinkage occurs depending on the
local thermal gradients and alloy...The shrinkage and local
solidification generates separation between the sensing elements and the
heaters...These then can cause a decoupling between the sensor and the
heaters as the heaters try to liquefy the slurry/solid solder mix
causing solder phase separation and voiding in the solder pot...This
then forces the heaters to higher power level until the sensor is in
full thermal conduction with the heaters... Then the heaters and their
attached thermal mass will have to "cool down" to the controller's set
point...
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
Sent: Thursday, September 02, 2010 8:37 AM
To: [log in to unmask]
Subject: Re: [TN] Wave Temperature Overshoot
We have the same wave and I have never seen any temperature shoot
overshoot. The temperature reading increases to 520F and stays constant
at that valve from a cold start. Takes about 3 hours from room temp to
reach 520F.
Amol S. Kane
Process Engineer
Catalyst Manufacturing Services
941 Route 38
Owego NY 13827
Office : 607-687-7669 X349
Fax : 607-687-9733
E-mail: [log in to unmask]
??Please consider the environment before printing this e-mail
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard D. Krug
Sent: Thursday, September 02, 2010 8:34 AM
To: [log in to unmask]
Subject: Re: [TN] Wave Temperature Overshoot
I'd suggest talking with Electrovert for recommendations on changing PID
controller settings.
You've got me thinking about additional cost savings here. We use the
timer functions to turn off the solder pot heaters at night and then
turn then back on in the morning. We turn on the heaters at 2:00 AM
M-F, even when pot may have been off all weekend. Pot always is ready
for production at 7:00 AM.
I'm going to record pot temperature for a week to see what actual
temperatures are. I may have a temperature overshoot but have never
seen it based on our warm up timer settings. A record of actual
overshoot could provide insight into PID controller setting changes.
Dick Krug, CSMTPE
SMT Process Engineer
Sparton Corporation
30167 Power Line Road
Brooksville, FL 34602-8299
p (352) 540-4012 (Internal Ext. 2012)
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rex Waygood
Sent: Thursday, September 02, 2010 7:41 AM
To: [log in to unmask]
Subject: [TN] Wave Temperature Overshoot
The following problem is on an Electovert Vectra with SN100C alloy.
Due to a decision to allow the bath to cool over night, to save energy,
we are experiencing over temperature shoot for several hours after
reaching temperature. Once the overshoot has gone the bath then seems to
control OK.
The PID controller for the bath has the same terms in it as it had for
SnPb.
If I make an assumption that SN100C is 100% Sn in terms of its Specific
Heat then I have 0.244 J/gm/K vs. 0.180 J/gm/K for 60/40 Sn/Pb. (1.36:1)
This is a big difference in specific heat.
Intuitively I feel that the SN100C should be less likely to overshoot.
Does anyone have experience of having to have the PID terms adjusted in
their wave having changed the alloy in order to maintain temperature?
Has anyone done the arithmetic to show that allowing the alloy to go
through a phase change in cooling down is more economic than just
keeping it above the phase change point? Again my intuition says it is
better to let it cool but I've been asked justify my assumption! :-)
Regards
Rex
Rex Waygood
Technical Manager
Hansatech EMS provides value manufacturing through engineering and
quality
Hansatech EMS Limited
Benson Road
Nuffield Industrial Estate
Poole
Dorset
BH17 0RY
+44 (0)1202 338200
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
WARNING: Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the
Export
Control Laws of the U.S. Government. Transfer of such data by any means
to a
foreign person, whether in the United States or abroad, without proper
export
authorization or other approval from the U.S. Department of State is
prohibited.
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
========================================================================
======
This email and any attachments thereto may contain private,
confidential, and
privileged material for the sole use of the intended recipient. Any
review, copying,
or distribution of this email (or any attachments thereto) by others is
strictly prohibited.
If you are not the intended recipient, please contact
[log in to unmask]
immediately and permanently delete the original and any copies of this
email and
any attachments thereto.
========================================================================
======
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
========================================================================
======
This email and any attachments thereto may contain private,
confidential, and
privileged material for the sole use of the intended recipient. Any
review, copying,
or distribution of this email (or any attachments thereto) by others is
strictly prohibited.
If you are not the intended recipient, please contact
[log in to unmask]
immediately and permanently delete the original and any copies of this
email and
any attachments thereto.
========================================================================
======
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|