Phil,
I was kinda surprised to see that a 1,1,1 product was still on the
market. Anyhow, we tin our gold plated connector leads using RMA fluxes. We
use a Chemtronics product called Flux-Off CZ for rosin flux removal. This is
an environmentally friendly material and works terrific. It is, however,
very expensive. It runs about $18 per can and over $300 per gallon when
using the liquid. Needless to say, I keep a tight lid on usage and only use
the material when absolutely neccessary (like cleaning tinned connectors).
Otherwise we use isopropyl alcohol for general benchtop cleaning operations.
Bill Kasprzak
Moog Inc.
> -----Original Message-----
> From: Phil Nutting [SMTP:[log in to unmask]]
> Sent: Friday, August 25, 2000 2:31 PM
> To: [log in to unmask]
> Subject: [TN] board cleaners
>
> Hi TechNetters
>
> For hand spot cleaning of PWBs we currently use a Miler-Stephenson product
> MS-195/CO2 which contains 1,1,1 Trichloroethane. I'm considering changing
> to a newer Ozone friendly material. Are there any recommendations for an
> aerosol package of board cleaner (using rosin flux at the moment)? Or
> recommendations of what NOT to buy? The stuff we use works very well but
> I'm trying to come into the new millinneum with many of our processies.
> Yikes... change!
>
> Reagrds,
>
> Phil Nutting
> Manufacturing Engineer
> Kaiser Systems, Inc.
> 126 Sohier Road
> Beverly, MA 01915
> ph: 978-922-9300
> fx: 978-922-8374
> [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|