TECHNET Archives

August 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
David Hillman <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Date:
Mon, 10 Aug 2015 07:52:11 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (45 lines)
Hello Ricardo - as long as the gold thickness of the thermal plane is thin
enough that you will not have a solder joint gold embrittlement situation
occur then soldering the thermal plane should not be an issue. In fact,
having an as-plated surface rather than a pretinned surface would be
significantly more manufacturing friendly and therefore favored.

Dave Hillman
Rockwell Collins
[log in to unmask]


On Fri, Aug 7, 2015 at 2:25 PM, Ricardo Moncaglieri <
[log in to unmask]> wrote:

> Estimated colleagues,
> In some cases componentĀ“s thermal planes Au finished which will be
> solded on ENEPIG TMM10 pcb where coplanarity is very critical then
> pretining modify undesirably coplanarity.
> Taking into account this fact, we have reflowed the component (solder
> the earth plane to pcb) without pretining and compare soldering under RX
> to another done with pretining. Have found out no difference between
> both cases (with and without pretining).
> Furthermore will run some tracking tests to verify joint.
>
> My question:
>
> Do you know or have any background experience on soldering Au finished
> thermal planes without pretining?
> In all other cases of Au components terminals finished, we always
> remove Au.
>
> brgds,Ricardo
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2