TECHNET Archives

June 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Braddock, Iain (UK)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Braddock, Iain (UK)
Date:
Thu, 28 Jun 2012 07:49:33 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (107 lines)
Louis,

I would very much appreciate a copy.

Thanks in advance.

	Iain 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of lee Hitchens
Sent: 28 June 2012 02:35
To: [log in to unmask]
Subject: Re: [TN] Chemtronics Konform SR Conformal Coating

                       *** WARNING ***
This mail has originated outside your organization, either from an external partner or the Global Internet.
Keep this in mind if you answer this message.
 
 

Hi Louis

May I have copy please.

Best Regards

Lee Hitchens
Technical Director

SCH Technologies is a Division of SCH Services Limited
Mob: +44 (0) 7862 25 33 21 www.conformalcoating.co.uk

TECHNICAL SUPPORT SERVICE
 
SCH Services Ltd offers a Technical Support Helpline to help address all issues relating to reliability. This includes contamination testing, cleanliness and cleaning issues, plus any coating related questions.
Please contact us via email or telephone:
 
[log in to unmask]   +44 (0)1226 249019 (office hours & answerphone)   +44
(0)7862 253321 (out-of-hours emergency)

The opinions expressed in this e-mail are strictly those of the sender and not of SCH Services Limited. This communication may contain information which is confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). Unauthorised use, copying or disclosure of any of it may be unlawful. If you are not the intended recipient(s) please note that any distribution, copying or use of this communication or the information in it is strictly prohibited. If you have received this communication in error please notify us by e-mail or by telephone (+44
(0)1226 249019) and then delete the e-mail and any copies of it. Virus Warning - Although steps have been taken to ensure that all email and attachments are virus-free, we cannot guarantee nor be held liable.
 
Company Registration: 04043334
Registered office: SCH Services Limited Newburgh Building McLintock Way Barnsley South Yorkshire S70 6BF




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Louis Hart
Sent: 27 June 2012 22:29
To: [log in to unmask]
Subject: Re: [TN] Chemtronics Konform SR Conformal Coating

Amol, If you want, have a look at a short technical paper I put in the August  2002 IPC Review, describing the experimentation done to set up an automated conformal coater. Summer of 2010 that authority Doug Pauls looked at it and did not recommend putting it in the trash, so it may have some worthwhile ideas. The website IPC archives for that publication do not go back to 2002. Let me know if you want to see it and I will dig up a copy.
Louis Hart

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
(Asteelflash,US)
Sent: Wednesday, June 27, 2012 7:55 AM
To: [log in to unmask]
Subject: [TN] Chemtronics Konform SR Conformal Coating

Dear Technetters,

I am being tasked to setup the above coating with the PVA automatic spray/dispense machine (fine spray head and the needle dispense head).
The coating comes in two forms, the Konform SR and Konform SR High viscosity, and some mixing is involved to arrive at the optimal viscosity. I plan to talk to PVA and get their expertise in setting up the machine and eventually setting up a DOE to determine the optimal viscosity specification limits. However I wanted to know if there are any techentters already spraying this coating thru automated conformal coating equipment. I was hoping to talk to someone who is willing to share his/her experience with this coating and hopefully obtain information on some "good" starting values

 

Thanks,

Amol

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


********************************************************************
This email and any attachments are confidential to the intended recipient and may also be privileged. If you are not the intended recipient please delete it from your system and notify the sender. You should not copy it or use it for any purpose nor disclose or distribute its contents to any other person. 

MBDA UK Limited, a company registered in England and Wales, registration number 3144919 whose registered office is at Six Hills Way, Stevenage, Hertfordshire, SG1 2DA, England.

********************************************************************


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2