Ron,
It is not so much that we can't use flux, it is just that we are set up for OA flux only. Our board washer uses only DI water. My assemblers have been using our OA liquid flux to aid in heat transfer and wicking, but they all agree that nothing is as good as our old Rosin flux wick.
Phil
-----Original Message-----
From: Dieselberg, Ron [mailto:[log in to unmask]]
Sent: Tuesday, November 12, 2002 3:42 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Wick
Phil, you have a unique problem. I would suggest that if you can't use flux that you would be better off just using a suitably sized stranded plated copper wire without any flux.
Ron Dieselberg
Trainer/Auditor
CMC ELECTRONICS
CINCINNATI
[log in to unmask]
-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: Tuesday, November 12, 2002 12:46 PM
To: [log in to unmask]
Subject: [TN] Solder Wick
Of the many brands and styles of solder wick on the market, with which one have you had the best luck?
Our specific needs are for non-fluxed wick. Rosin or no-clean flux are not acceptable in our system.
Thanks in advance,
Phil Nutting
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|