TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 14 Aug 1998 08:10:07 -0500
Content-Type:
multipart/mixed
Parts/Attachments:
text/plain (544 bytes) , PIC15697.PCX (4 kB)
               (Embedded image moved to file: PIC15697.PCX)

From: Dennis J Fall@TFT on 08/14/98 08:10 AM


To:   [log in to unmask]
cc:
Subject:  10/90 solder to copper bonding

Are there any good ways to bond a high temp eutectic solder sphere
Sn10/Pb90 to copper without using solder paste or flux?

Dennis Fall                        P: 507-625-8445 x17

Engineer                           F: 507-625-3523

Thin Film Technology Corporation         mailto:[log in to unmask]

1980 Commerce Drive                http://www.thin-film.com

North Mankato, MN 56003-1702


ATOM RSS1 RSS2