TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Johannes Sivula <[log in to unmask]>
Date:
Wed, 19 Aug 1998 09:47:34 +0300
Reply-To:
"\"TechNet E-Mail Forum.\" <[log in to unmask]>, Johannes Sivula" <[log in to unmask]>
Parts/Attachments:
text/plain (54 lines)
You wrote:
"
Because of a vendor mis-hap we recieved pcbs with      palladium and not
tin plating.    We use a 2% silver solder so it is a good match.   We are
concerned with  any long term effects i.e. corrosion.
Can some of you please respond with your experience
with palladium and pcbs. Don Fumia  "

---------------------------------------------------------------------------
------------------------------------------------------------------
Hi,

We have made some preliminary trials with Palladium Process called "
electroless palladium "
by Atotech, with  formic acid as the reducing agent.

I suppose there is also a process called " immersion  palladium ".
Personally I think it gets too
thin and it is preferrably used as a activator in  Ni/Au- processes, for
example.

Well, in our case it worked fine, we are pleased with solderability. We
have not made environmental tests
& other tests so far, personally I think that corrosion is not a problem,
because palladium is the most
noble metal and hence it is almost impossible to get it corrode.

The real problem of palladiumin our case is availibility/price fluctuation
in Europe.
Brs, Johannes

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2