January 6, 2008
If the solder flux used is RMA or equivalent, is there any real benefit to
doing a cleanliness test? I have reviewed OEM cleanliness test resords at
several OEMs and the data I reviewed shows folks rarely, if ever fail this
test.
>From: Graham Collins <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
>To: [log in to unmask]
>Subject: Re: [TN] specifying board cleanliness
>Date: Thu, 3 Jan 2008 11:09:58 -0400
>
>Happy New Year Phil!
>Well, "it depends"...
>
>First question is how clean do you need them to be? Depends on the
>application and environment. Second question is what sort of assembly
>process the CM is using - if "no clean" then they will be justifiably
>opposed to cleanliness testing.
>
>The generic callout that we most commonly see on drawings is "clean per
>J-STD-001 C-22" - which translates into clean the assembly, both sides,
>and then do an ionic contamination test with a upper limit of 1.56
>micrograms / cm2 NaCl equivalent contamination. I'm not sure why
>J-STD-001 gives an option to only clean one side - never seen that
>process in use. Anyway, a starting point...
>
>regards,
>
>Graham Collins
>Halifax Production Engineering
>L-3 communications Electronic Systems
>(902) 873-2000 ext. 6215
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
>Sent: Thursday, January 03, 2008 10:45 AM
>To: [log in to unmask]
>Subject: [TN] specifying board cleanliness
>
>Good Morning and Happy New Year to All,
>
>Let me start by confessing my ignorance relative to cleanliness of
>circuit boards. We have no idea what numbers to specify that fit into
>the IPC testing methods for board cleanliness. If I tell my CMs to make
>the boards clean, it would be good to specify a target value and or test
>method.
>
>Can someone give me some guidance on how to chose these specifications?
>What are worth while tests and which ones are window dressing?
>
>I've read through some of the IPC tests methods and my head hurts.
>
>Thanks in advance,
>
>Phil Nutting
>
>Note: All the information contained in this e-mail and its attachments
>is proprietary to Kaiser Systems, Inc. and it may not be reproduced
>without the prior written permission of sender. If you have received
>this email in error, please immediately return it to sender and delete
>the copy you received.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>archives of previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|