hello technet

the mostly discussed problem of the plasic range of 60/40 solder can be
answered in two statements

--- the eutectic point is at 61.9 weight percent tin (Thaddeus B Massalski
Binary Alloy Phase        Diagrams ASM)
--- binary phase diagrams show the constitution of alloys at the
equilibrium
    after a very slow cooling rate
    during a technical cooling (soldering) the cooling speed is so high
that you cannot notice a      plastic range. 

Karl Ring
ZVE 

 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2