Hi Technet,
I'm looking for an adhesive that can be used for keeping heavy components in place during double sided reflow soldering. Up to now we're using PC-flexmask (the latex-type mask that is normally used for wave soldering) but this material needs a couple of hours to cure, and cannot withstand the cleaning of intermediate paste-misprints.
The adhesive should have following properties :
- fast curing, preferably at room temperature.
- withstanding soldering temperatures and cleaning (in aliphatic hydrocarbon solvent)
- easy to remove after assembly, although visible residues are acceptable
- adhering to plastic and ceramic parts, and to solderresist
- nonconductive, non corrosive
Any suggestions ?
Daan Terstegge
Signaal Communications
* Unclassified *
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|