Vickie:
We purchased one of the original wavesolder anlayzers and collected
some really good data on our machine (HOLLIS GBS). A few months back
we purchased a wavesolder optimizer. The Optimizer is a good tool to
check what you machine is doing after you have optimized with DOEs and
profiling CCAs. The new optimizers or capable of checking both chip
and main waves. I believe it's a good tool, even if you have the
newer digitally controlled machines (SOLTEC DELTA SYSTEM). This
second generation Wave Solder Optimizer is a good follow-up by Martin
Ingall.
Ron H.