Usually a sacrificial gold is the final finish over the nickel. The fluxes used to solder to nickel are unique. IMHO, no-cleans; not allowed.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Thursday, August 29, 2013 12:01 PM
To: [log in to unmask]
Subject: Re: [TN] Solder joint failure
In my experience nickel is NOT easy to solder to at all.
-----Original Message-----
From: Victor Hernandez [mailto:[log in to unmask]]
Sent: Thursday, August 29, 2013 2:53 PM
To: [log in to unmask]
Subject: [TN] Solder joint failure
Fellow TechNetters:
Should I be concern with an electroless matted nickel plating over an aluminum sheet metal surface and solder onto a copper heat tube? I recall something about directly soldering onto a nickel surface. Beside nickel oxidation. Any suggestions would be greatly appreciated.
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|