TECHNET Archives

February 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Genny Gibbard <[log in to unmask]>
Date:
Fri, 9 Feb 2007 22:08:47 +0100
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "P. Langeveld" <[log in to unmask]>
Subject:
From:
"P. Langeveld" <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (43 lines)
What we did with expired solder paste: add 100 ml of a mixture of IPA
and Butyl-Acetate 1:1, stirr and pour the overlaying liquid in your
organic waste bin. Do it twice. Leave the remaining solder drying.
Then the dryed solder can be melted in your wave solder pot without
much fuming or spattering.

Success.
Soft Soldering Processes
Peer Langeveld, Consultant
The Netherlands

2007/2/9, Genny Gibbard <[log in to unmask]>:
> Was sorting through the fridge in the stockroom at work...pushed aside a
> couple of sandwiches and yogurts (the stockroom people keep their
> lunches in there...) and came across a box with 9kg(18 jars) of solder
> paste expired in mid 2004 - a brand we don't use any more.  Standard
> 63/37 no-clean.
>
> What would you do with it?  Never even been opened.
>
> Genny.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2