Victor,
the stencil apertures are related to the pitch and not necessarily to the pad width. For a 0.281mm wide pad, I assume you have a 0.5mm pitch. IPC-7525 recommends a 0.25mm wide aperture.
Of course, the reliability is a function of the volume of solder, so if you have no other funkier parts, like 0201, leadless, 16mils pitch, I suggest you used a 6 mils thick stencil.
Regards,
Ioan
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Victor G. Hernandez
Sent: Tuesday, September 11, 2007 3:32 PM
To: [log in to unmask]
Subject: [TN] LF Solder Paste Stencil Volume
Fellow TechNetters:
What is the guideline/require for solder paste application onto a pad
with the following dimensions:
Length: 2.213 mm and Width: 0.281 mm. A gull wing device will be
placed at this location.
Victor,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|