TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Mon, 11 Aug 2008 07:52:19 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (86 lines)
Hi again Inge,

The report is posted:

http://stevezeva.homestead.com/files/Electroless_Report.doc

It's a 6MB file, so be patient during download...

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Monday, August 11, 2008 6:32 AM
To: [log in to unmask]
Subject: Re: [TN] looking for ENiG photos

Pete,

I happened to find one of my old reports from 2001. Just few pages about
difference between Dark ENIG pads, Pale and Grey dittos.  Sending to Dr
Gregory's clinic for analysis. He may find them operable. Wait and see.

Inge



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete Houwen
Sent: den 22 juli 2008 21:38
To: [log in to unmask]
Subject: Re: [TN] looking for ENiG photos

Thanks, everyone, for all your help.  This has been exasperating.

Thankfully, I won't need to exaggerrate (though I hadn't planned to, I
just applied hyperbole when I said I might)

Looking at things other than the weird plating, after we did our
research and site visit, it turns out they brokered the boards out
anyway, used different laminate than they promised, gave us one
microsection from a different lot than they shipped, the microsection on
the other board showed lots of nailheads and layer separation, there was
soldermask residue all over the pads.... I just hope purchasing
understands enough of the "technical"
infomation to realize how much this cost savings would cost us.  Of
course, months ago when I pointed out they admitted they couldn't even
meet our specs, it didn't stop anything.

Pete

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2