Not only that, but it is inevitable that manufacturer X will blame the
product of manufacturer Y, should you ever run into any trouble.
Brian
Karen Tellefsen wrote:
> Do solder manufacturers actually develop products to be used together by
> matching chemistries?
>
> Sometimes.
>
> Should one attempt to utilize paste, wire, and liquid flux all from a
> single supplier, or is there no value there, in that an ORH0 is an ORH0 is
> an ORH0?
>
> The advantage using one vendors chemistries is that the vendor may have
> tested the materials together and can provide compatability/reliability
> data. If you use chemistries from different vendors, you'll have to do
> any compatability testing yourself.
>
> Karen Tellefsen - Electrical Testing
> [log in to unmask]
> 908-791-3069
>
>
>
>
> "Glidden, Kevin"
> <Kevin.Glidden@as
> tronics.com> To
> TechNet E-Mail Forum
> 04/20/2010 06:56 <[log in to unmask]>, Karen Tellefsen
> AM <[log in to unmask]>
> cc
>
> Subject
> RE: [TN] Flux-Cored Wire Solder:
> Halide / Halide-Free
>
>
>
>
>
>
>
>
>
>
> Karen and Guy,
>
> Thanks for the responses. I like the looks of the Aqualine...
>
> But, more questions comes to mind.....
>
> Do solder manufacturers actually develop products to be used together by
> matching chemistries?
>
> Should one attempt to utilize paste, wire, and liquid flux all from a
> single supplier, or is there no value there, in that an ORH0 is an ORH0 is
> an ORH0?
>
> For example, in some wire solder data sheets you will see statements that
> it uses the same flux chemistry as either a paste or a liquid flux from the
> same manufacturer. But on the other hand, I have seen manufacturers state
> that the compatible flux with a given paste in product X, but then the
> datasheet for product X states it was developed with the same chemistry as
> a completely different paste.
>
> Thanks,
>
> Kevin Glidden
> Manufacturing Engineer
> Astronics Luminescent Systems Inc.
>
> -----Original Message-----
> From: Karen Tellefsen [mailto:[log in to unmask]]
> Sent: Monday, April 19, 2010 4:59 PM
> To: [log in to unmask]
> Subject: Re: [TN] Flux-Cored Wire Solder: Halide / Halide-Free
>
> Aqualine 6000 is halide-free, ORH0. Must be washed, washable in hot DI
> water.
>
> Karen Tellefsen - Electrical Testing
> [log in to unmask]
> 908-791-3069
>
>
>
>
> "Guy M. Ramsey"
> <gramsey@RDCIRCUI
> TS.COM> To
> Sent by: TechNet [log in to unmask]
> <[log in to unmask]> cc
>
> Subject
> 04/19/2010 02:42 Re: [TN] Flux-Cored Wire Solder:
> PM Halide / Halide-Free
>
>
> Please respond to
> TechNet E-Mail
> Forum
> <[log in to unmask]>
> ; Please respond
> to
> "Guy M. Ramsey"
> <gramsey@RDCIRCUI
> TS.COM>
>
>
>
>
>
>
> Amtech makes a wire core solder with Halide free watersoluble flux. You
> should
> clean it but it cleans fairly easily. If you are looking to change your
> cleaning
> process, I recommend you look at it. We clean it with a spot steam cleaner.
>
>
> If you are staying with alcohol you cannot use it.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|