     Kristian,
       I am not sure of the thru-put you need, but a very interesting 
     system is the Panasonic SoftBeam System, which meets the requirement 
     of "a functional simple selective soldering system". 
     Call your local Panasonic rep, or Tom Bradfish at (USA) 847-288-4400. 
     Tell 'em Jeff Hempton sent ya....after they are done laughing, they 
     will be able to help you   ;')....Regards.
     
     United Technology Electronic Controls
     Jeff L. Hempton, Sr. SMD Engineer




______________________________ Forward Header __________________________________
Subject: [TN] Automated Selective Soldering
Author:  Kristian Fohlin-Svensson <[log in to unmask]> at Internet
Date:    3/1/99 3:36 PM


Hi TechNetters !
Is there anybody out there who knows where to find a functional simple 
selective soldering system. We are now running a small Inertec module but 
need some more capacity. I am awere of the Inertec and the Ersa selective 
soldering systems, but that is not exactely what I need. I am pretty 
satisfyed with the Inertec module but it could be alot better.
     
So long
Kristian Fohlin-Svensson
PartnerTech AB
S-597 80 Åtvidaberg
E-mail: [log in to unmask] 
Tel: +46 (0)120 816 58
Fax: +46 (0)120 122 02
     
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c 
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name> 
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for 
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 
ext.312
################################################################
     
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2