TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 13 Jul 2009 14:53:21 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
From:
Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
Lee,

If you are talking room temperature measurement, then a good, non-contact CMM will do nicely. At elevated temperatures Moire and Digital Image Correlation (DIC) methods can be employed. 

Bev



________________________________



From: Lee parker <[log in to unmask]> 

To: TechNet E-Mail Forum <[log in to unmask]>; Bev Christian 

Sent: Mon Jul 13 14:37:02 2009

Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB 





Bev and Richard

 

How do you suggest we measure to local bow and twist?

 

Best regards

Lee

J. L. Parker Ph. D.

JLP Consultants LLC

804 779 3389



	 

	----- Original Message ----- 

	From: Bev Christian <mailto:[log in to unmask]>  

	To: [log in to unmask] 

	Sent: Monday, July 13, 2009 12:53 PM

	Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB



	Richard,

	Correct as usual, Richard. This was always a big deal at Nortel where completed circuit packs would have to be slotted into card cages. 

	Bev

	On vacation

	

	----- Original Message -----

	From: Stadem, Richard D. <[log in to unmask]>

	To: [log in to unmask] <[log in to unmask]>; Bev Christian

	Sent: Mon Jul 13 11:06:30 2009

	Subject: RE: [TN] Maximum Allowable Bow & Twist for PWB-PCB

	

	Bev, I totally agree with you, but the point they are getting at in IPC

	2221 is that no section of the PWB should have more than .75% per inch

	as a rate of warpage, extending in both the X and Y directions, after

	reflow. This is because if you have more warpage than that you are

	putting a stress on the resultant solder joints that leads to a

	reduction in reliability, especially with a lead-free joint and also

	especially if you need to straighten the CCA when mounting it into a

	chassis or frame.

	I think this specification, like so many others that were based on

	leaded solder, should be revisited for unleaded solders.

	

	-----Original Message-----

	From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian

	Sent: Friday, July 10, 2009 3:24 PM

	To: [log in to unmask]

	Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB

	

	I contend this is old school and if you aren't measuring warpage at

	reflow temperatures how do you know you aren't suffering from head on

	pillow?

	

	I suggest the term head in pillow be dropped because you don't actually

	put your head IN a pillow.

	

	Bev

	RIM

	

	PS Waiting for my Dewism.

	

	-----Original Message-----

	From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard

	Sent: Friday, July 10, 2009 4:20 PM

	To: [log in to unmask]

	Subject: Re: [TN] Maximum Allowable Bow & Twist for PWB-PCB

	

	IPC-2221 5.2.4 

	...

	Unless otherwise specified by master drawing, max bow and twist shall be

	0.75% for boards that use surface mount components and 1.5% for all

	other board technologies.

	...

	Values are measured as per IPC-TM-650 Method 2.4.22 

	

	

	Genny Gibbard, P. Eng 

	Manufacturing Engineer, Vecima

	PTS dept. x.4229 

	

	-----Original Message-----

	From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez

	Sent: July 10, 2009 2:15 PM

	To: [log in to unmask]

	Subject: [TN] Maximum Allowable Bow & Twist for PWB-PCB

	

	What is the maximum allowable Bow & Twist value?   Not able to locate in

	IPC-2221, 2222, & 6012A

	

	Victor,

	

	---------------------------------------------------

	Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

	unsubscribe, send a message to [log in to unmask] with following text in

	the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

	(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

	Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

	posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

	archives of previous posts at: http://listserv.ipc.org/archives Please

	visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

	additional information, or contact Keach Sasamori at [log in to unmask] or

	847-615-7100 ext.2815

	-----------------------------------------------------

	

	---------------------------------------------------

	Technet Mail List provided as a service by IPC using LISTSERV 15.0

	To unsubscribe, send a message to [log in to unmask] with following text

	in

	the BODY (NOT the subject field): SIGNOFF Technet

	To temporarily halt or (re-start) delivery of Technet send e-mail to

	[log in to unmask]: SET Technet NOMAIL or (MAIL)

	To receive ONE mailing per day of all the posts: send e-mail to

	[log in to unmask]: SET Technet Digest

	Search the archives of previous posts at:

	http://listserv.ipc.org/archives

	Please visit IPC web site

	http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

	information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

	ext.2815

	-----------------------------------------------------

	

	---------------------------------------------------------------------

	This transmission (including any attachments) may contain confidential

	information, privileged material (including material protected by the

	solicitor-client or other applicable privileges), or constitute

	non-public information. Any use of this information by anyone other than

	the intended recipient is prohibited. If you have received this

	transmission in error, please immediately reply to the sender and delete

	this information from your system. Use, dissemination, distribution, or

	reproduction of this transmission by unintended recipients is not

	authorized and may be unlawful.

	

	---------------------------------------------------

	Technet Mail List provided as a service by IPC using LISTSERV 15.0

	To unsubscribe, send a message to [log in to unmask] with following text

	in

	the BODY (NOT the subject field): SIGNOFF Technet

	To temporarily halt or (re-start) delivery of Technet send e-mail to

	[log in to unmask]: SET Technet NOMAIL or (MAIL)

	To receive ONE mailing per day of all the posts: send e-mail to

	[log in to unmask]: SET Technet Digest

	Search the archives of previous posts at:

	http://listserv.ipc.org/archives

	Please visit IPC web site

	http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

	information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

	ext.2815

	-----------------------------------------------------

	

	---------------------------------------------------------------------

	This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

	

	---------------------------------------------------

	Technet Mail List provided as a service by IPC using LISTSERV 15.0

	To unsubscribe, send a message to [log in to unmask] with following text in

	the BODY (NOT the subject field): SIGNOFF Technet

	To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

	To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

	Search the archives of previous posts at: http://listserv.ipc.org/archives

	Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

	-----------------------------------------------------

	





---------------------------------------------------------------------

This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.


ATOM RSS1 RSS2