TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 8 Jan 2008 12:49:24 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Herminia Guevarra <[log in to unmask]>
Subject:
From:
Herminia Guevarra <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (98 lines)
I need it too...Thanks

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez
Sent: Tuesday, January 08, 2008 12:17 PM
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] Warpage of components

Can this warpage calculation be shared with other like my self?

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord
Sent: Tuesday, January 08, 2008 9:56 AM
To: [log in to unmask]
Subject: [TN] SV: [TN] Warpage of components

I promised a simple warpage calculation formula, if not too many, I'll send
offline...
Inge

-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Werner Engelmaier /*
Skickat: den 8 januari 2008 14:15
Till: [log in to unmask]
Ämne: Re: [TN] Warpage of components

HI Ingemar,
Well said.
A warpage criterion for components would have to be based on a total 
out-of-plane measurement at soldering temperatures. This non-coplanarity
measure would 
have to be about the thickness of the solder paste layer to avoid solder 
opens, and it would have to be based on the total final solder joint
thickness to 
avoid solder joint cracking due to warpage tensile loads on cooling from 
reflow.

Werner



**************
Start the year off right.  Easy ways to stay in shape.
     
http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

8/1/2008NOT INTENDED AS A SUBSTITUTE FOR A WRITING 

NOTHING IN THIS E-MAIL, IN ANY E-MAIL THREAD OF WHICH IT MAY BE A PART, OR IN ANY ATTACHMENTS THERETO, SHALL CONSTITUTE A BINDING CONTRACT, OR ANY CONTRACTUAL OBLIGATION BY PNY, OR ANY INTENT TO ENTER INTO ANY BINDING OBLIGATIONS, NOTWITHSTANDING ANY ENACTMENT OF THE UNIFORM ELECTRONIC TRANSACTIONS ACT, THE FEDERAL E-SIGN ACT, OR ANY OTHER STATE OR FEDERAL LAW OF SIMILAR SUBSTANCE OR EFFECT.  THIS EMAIL MESSAGE, ITS CONTENTS AND ATTACHMENTS ARE NOT INTENDED TO REPRESENT AN OFFER OR ACCEPTANCE OF AN OFFER TO ENTER INTO A CONTRACT.  NOTHING IN THIS E-MAIL, IN ANY E-MAIL THREAD OF WHICH IT MAY BE A PART, OR IN ANY ATTACHMENTS THERETO SHALL ALTER THIS DISCLAIMER.  

This e-mail message from PNY Technologies, Inc. is for the sole use of the intended recipient(s) and may contain confidential and privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply e-mail and destroy all copies of the original message. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2