I have been battling SMT ceramic capacitor cracking problems for a while, as
I am sure most of you have.  I am experiencing cracking from mechanical and
most likely thermal stress as well.  I have addressed many of these issues
(depanelization, profile, etc...) using literature from MLC manufacturer's
technical information.  I am now looking for a general capacitor size vs.
strength data for various stresses.  I know that generally larger parts are
more likely to have problems but for each size of cap it is difficult to
compare.  I have looked at RAC data as well as IPC, and have not found
anything exactly like what I am looking for.

Does anyone know of a source of such information or the best place to start
compiling a list of my own?

Any suggestions would be appreciated.

Thanks

David Romero

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2