TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Sat, 1 May 1999 20:57:21 -0400
Content-Type:
text/plain; charset="us-ascii"
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, joyce <[log in to unmask]>
Parts/Attachments:
text/plain (54 lines)
years ago, I used a micro section device. (you may find it at display
section of MRS conference).  If I remember correctly, it was invented by IBM
and marketed by a third party (sorry, can't remember the name).  The device
has three micrometers mount on a stand.  The position pin can be adjusted to
a level which the material required to be removed (plane of interests).
Three "stop posts" prevent the sample to be over grinded/polished.  I used
the device once or twice. You can section the sample to particular line on
fan-out pattern of to an IC circuit ( > few micron).  X-ray photo with
"clear moulding compond" are helpful to position the area of interest.  The
microsection job was not easy, but the device made it a little bit tolerable.
jk
At 01:59 PM 4/30/99 EDT, you wrote:
>Hans
>If you find such a system be certain to alert the world.
>
>What you aret alking about is called a human being.  One that can look at the
>section at incremental grinds and determine where they are in relation to what
>is needed.
>
>All automated systems go to a preset location and you get what is at
>that preset location.  Hence the need to have an alignment system to put
>what you want at the right location.
>
>Susan Mansilla
>Technical Director
>Robisan Lab
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2