TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Rex Waygood <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Rex Waygood <[log in to unmask]>
Date:
Wed, 18 Jun 2008 15:00:24 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (74 lines)
I've read the thread with interest.
In the UK PPE is a last resort and should not be used until all other
avenues for preventing exposure of operators has been explored.
In the UK the requirements for PPE use, monitoring, training, logging
etc are not trivial.
From one of your subsequent comments we would explore other materials,
changing the process, better extraction etc before resorting to PPE.


Rex Waygood
Technical Manager
 
PartnerTech Poole Ltd 
Benson Road
Poole
Dorset BH17 0RY
United Kingdom
 
Tel: +44 (0)1202 674333
Fax: +44 (0)1202 678028
DDI: +44 (0)1202 338222
Mob: +44 (0)7887 997403
 
[log in to unmask]
www.PartnerTech.co.uk

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: 17 June 2008 14:56
To: [log in to unmask]
Subject: [TN] Respirator Cartridge for IPA

I have an unusual question for all you chemical types out there.

We are doing some heavy cleaning with IPA and our organic vapor
cartridges on the respirator masks don't seem to keep the smell of the
IPA away from the operator. According to the different data sheets I've
looked at say that an organic vapor cartridge should work.

My question is can you still smell the fragrance of the IPA while having
all the bad stuff trapped by an organic vapor cartridge? If so how would
you know when the cartridge was saturated?

Thanks,

KennyB

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

-------------------------------------------------------------------------------

The information contained within this e-mail and any attachments contained therein may be confidential and/or legally privileged and is for the use of the intended recipient only. If you are not the intended recipient please delete it from your system and notify the sender by return e-mail. The content of this e-mail may not be copied or disclosed to any third parties without prior permission from the sender. 

 

E-mail is susceptible to data corruption, interception, tampering and viruses. We do not accept any liability for any such incidents or any consequences thereof.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2