TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Mon, 14 Jul 2008 13:39:21 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (93 lines)
Vladimir
Here are potential causes of MLCCC cracking, and how to tell what caused
the crack based on the crack's position, run direction, etc.
http://www.ami.ac.uk/courses/topics/0179_fmcc/index.html#3

http://www.syfer.com/category_docs/AN0005_Mechanical_Cracking.pdf

And an authorative paper on the subject by John Maxwell, who I think
knows more about root causes of cap cracking than anyone:

http://www.avx.co.il/docs/techinfo/cracks.pdf 

And a potential solution to the problem:

http://www.avx.co.il/docs/techinfo/mlccflex.pdf

Qualify it first.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir
Sent: Monday, July 14, 2008 1:13 PM
To: [log in to unmask]
Subject: Re: [TN] Ceramic caps

Well, in the case I was asking about none of the failures were in that
direction (across the body) but always along it splitting both ends in
half either vertically or horizontally. Still a puzzle to me :-)

Regards,

Vladimir

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Monday, July 14, 2008 2:05 PM
To: [log in to unmask]
Subject: Re: [TN] Ceramic caps

Right!

KennyB
-----Original Message-----
From: Igoshev, Vladimir [mailto:[log in to unmask]]
Sent: Monday, July 14, 2008 10:48 AM
To: TechNet E-Mail Forum; Ken Bloomquist
Subject: RE: [TN] Ceramic caps

So they were cracking normal to, not along the body of the caps. Right?

Regards,

Vladimir


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2