Mike,
HumiSeal 1063 and 1071 Strippers work a treat on the DCA coating.
Both materials are available in gel forms for localised rework, or liquid form for complete immersion stripping.
Please contact me offline if you require any further details etc.
Best Regards,
Phil Kinner
Chief Chemist
Please note that Concoat has recently acquired the former Multicore SPCID business. For more information, please visit our new web site www.concoatsystems.com
Concoat Ltd
Alasan House, Albany Park,
Camberley, Surrey, GU16 7PH
Tel: +44 (0) 1276 691100
Fax: +44 (0) 1276 691227
Attention: This message is for the named person's use only. It may contain confidential, proprietary or legally privileged information. No confidentiality or privilege is waived or lost by any mistransmission. If you receive this message in error, please immediately delete it and all copies of it from your system, destroy any hard copies of it securely and notify the sender. You must not, directly or indirectly, use, disclose, distribute, print, or copy any part of this message if you are not the intended recipient. Concoat Ltd and any of its subsidiaries each reserve the right to monitor all e-mail communications through its networks.
Any views expressed in this message are those of the individual sender, except where th
----- Original Message -----
From: Michael Bell
To: [log in to unmask]
Sent: Tuesday, June 11, 2002 9:21 PM
Subject: [TN] Electrolude DCA COnformal Coating Rework
Hi all,
Has anyone had any experiance in reworking PCA's that have Electrolube DCA
Conformal Coating applied to them???? I believe there is a form of rework
gel, that dissolves the coating in preparation for reworking, but I haven't
tried it, has anyone?????
Cheers
Mike
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|