TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0u3m9w-0000AWC; Mon, 1 Apr 96 10:08 CST
Encoding:
16 TEXT
Old-Return-Path:
Date:
Mon, 01 Apr 96 11:13:00 EST
Precedence:
list
Resent-From:
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/3240
TO:
"'IPC Technet Input'" <[log in to unmask]>
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"hRwMH3.0.7kE.G-_Nn"@ipc>
From [log in to unmask] Wed Apr 3 16:
47:51 1996
From:
"Dill, Norm J" <[log in to unmask]>
X-Loop:
Subject:
X-Mailer:
Microsoft Mail V3.0
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (19 lines)

    Our HASL solder thickness spec. is 0.3 to 1.5 mils.  Is it unreasonable 
to expect using a horizontal HASL process that 1.5 mils will be the actual 
max. on 100% of the pads on both sides of the board, even with fine pitch (< 
= 20 mils)?
    My guess is that the surface tension of the molten solder on the fine 
pitch pads, its low mass and the surrounding geography, make it difficult 
for the air knives to do consistant leveling.
    Some of our product mix here is Mil Spec work.  Converting the boards 
with fine pitch on both sides to Au/Ni may be more pain than it is worth.
    Any inputs on this subject will be greatly appreciated.