Ryan, not sure how much the capped vias increase cost. As far as
reliability, though, we've been using this design for many years in a
military avionics environment with good results.
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: Ryan Grant [SMTP:[log in to unmask]]
Sent: Friday, September 07, 2001 11:25 AM
To: [log in to unmask]
Subject: Re: [TN] Cap-plate Via-in-Pad??
Jim,
How has the cap plate filled via been working out on the production
line,
in terms or cost and reliability. We have had some customers
inquire about
the technology, but I don't have first hand knowledge.
Kind Regards
Ryan Grant
Advanced Technology Engineer
MCMS
(208) 898-1145
[log in to unmask]
> -----Original Message-----
> From: Marsico, James [SMTP:[log in to unmask]]
> Sent: Tuesday, September 04, 2001 9:01 AM
> To: [log in to unmask]
> Subject: Re: [TN] Cap-plate Via-in-Pad??
>
> This was probably referring to a filled via that was copper plated
over
> the
> top, resulting in what appears like a round, solid pad. We use
this
> design
> quite often.
>
> Jim Marsico
> Senior Engineer
> Production Engineering
> EDO Electronics Systems Group
> [log in to unmask] <mailto:[log in to unmask]>
> 631-595-5879
>
>
>
> -----Original Message-----
> From: Rick Thompson
[SMTP:[log in to unmask]]
> Sent: Tuesday, September 04, 2001 10:40 AM
> To: [log in to unmask]
> Subject: [TN] Cap-plate Via-in-Pad??
>
> Hi,
>
> I was doing some reading over the weekend and came across
a
> reference I
> wasn't familiar with that said:
> "Note that a filled and cap-plate via-in-pad
construction was
> used".
>
> Can someone enlighten me as to what 'filled and cap-plate
> via-in-pad' is?
>
> Thanks,
>
>
> Rick Thompson
> Ventura Electronics Assembly
> 2655 Park Center Dr.
> Simi Valley, CA 93065
>
> +1 (805) 584-9858 x-304 voice
> +1 (805) 584-1529 fax
> [log in to unmask]
>
>
>
--------------------------------------------------------------------------
> --
> -----
> Technet Mail List provided as a free service by IPC using
LISTSERV
> 1.8d
> To unsubscribe, send a message to [log in to unmask] with
following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
> message:
> SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line
Resources &
> Databases > E-mail Archives
> Please visit IPC web site
(http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask]
or
> 847-509-9700 ext.5315
>
>
--------------------------------------------------------------------------
> --
> -----
>
>
--------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> To unsubscribe, send a message to [log in to unmask] with following
text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
> ext.5315
>
--------------------------------------------------------------------------
> -------
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|