A word of caution:  Holes will normally plate shut closer to the surfaces,
leaving a barrel shaped hole with trapped plating solution.



----------
> From: [log in to unmask]
> To: [log in to unmask]
> Subject: [TN] Copper Plugging Vias
> Date: Tuesday, May 12, 1998 3:47 PM
>
>      Address,
>
>      How many suppliers are copper plugging .008 finish vias, provided
the
>      surface finish is OSP.  Provide your answer(s) on finished board
>      thicknesses of .062 and .028, std tolerances.  If so, what
percentage,
>      nominal, are you able to plug shut.  Through cross-sectioning do you
>      have the following conditions.
>
>      From my past experience the plugging of vias is not feasible using
an
>      electroless and electrolytic plating combination process.
>      Cross-sectioning would later show a dog-bone effect.  Does this
still
>      hold true today.
>
>      Thanks,
>
>      John Gulley
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2