TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ingemar Hernefjord (KC/EMW)
Date:
Mon, 2 Aug 2004 13:39:56 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (43 lines)
We have done FEA (NASTRAN, ANSYS) on BGA balls by means of what they call Maxwell's rheological elasticity model. May be possible to
share with you, Shean, if you are interested I can ask the guy who did this huge job a couple of years ago. You need a good math background to understand this report.

Ingemar Hernefjord
Ericsson Microwave Systems

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Shean Dalton
Sent: den 28 juli 2004 21:04
To: [log in to unmask]
Subject: Re: [TN] BGA pad missmatch


Hi Phil,

I have been hoping for a response from someone who has practical
experience with this, as it is interesting to me.  That said, I suspect
areas of concern would be for TCE.  The larger pad size takes away
solder from the bulk joint, effectively reducing the standoff height.
Again, I suspect the reduced standoff height might reduce the "flexure"
ability of the solder joint to "absorb" the TCE mismatch.    And, using
a larger sphere diameter may compensate for the large pad size,
effectively raising the standoff height.


 Sure would be nice to do a
finite elemental analysis.

Have fun!,

Shean Dalton
Austin American Technology

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2