We have done FEA (NASTRAN, ANSYS) on BGA balls by means of what they call Maxwell's rheological elasticity model. May be possible to
share with you, Shean, if you are interested I can ask the guy who did this huge job a couple of years ago. You need a good math background to understand this report.
Ingemar Hernefjord
Ericsson Microwave Systems
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Shean Dalton
Sent: den 28 juli 2004 21:04
To: [log in to unmask]
Subject: Re: [TN] BGA pad missmatch
Hi Phil,
I have been hoping for a response from someone who has practical
experience with this, as it is interesting to me. That said, I suspect
areas of concern would be for TCE. The larger pad size takes away
solder from the bulk joint, effectively reducing the standoff height.
Again, I suspect the reduced standoff height might reduce the "flexure"
ability of the solder joint to "absorb" the TCE mismatch. And, using
a larger sphere diameter may compensate for the large pad size,
effectively raising the standoff height.
Sure would be nice to do a
finite elemental analysis.
Have fun!,
Shean Dalton
Austin American Technology
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|