TECHNET Archives

August 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
"Morse, Carrie" <[log in to unmask]>
Date:
Thu, 29 Aug 2002 18:36:11 -0400
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Morse, Carrie" <[log in to unmask]>
Parts/Attachments:
text/plain (78 lines)
Dave,
Are the boards you are running double sided SMT?



-----Original Message-----
From: Dave Chapman [mailto:[log in to unmask]]
Sent: Thursday, August 29, 2002 4:01 PM
To: [log in to unmask]
Subject: Re: [TN] DDarkly comment re OSP vs White Tin, etc


We have been having great results with Immersion Silver as a drop in
replacement for our HASL and OSP product. 
Dave Chapman
Manufacturing Engineer
Circuit Service Inc.

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, August 29, 2002 12:53 PM
To: [log in to unmask]
Subject: [TN] DDarkly comment re OSP vs White Tin, etc


I agree that OSP has a lot of virtues and it has improved greatly in the
last 10 years.  Particularly in terms of storage, thermal cycles, less
dependence upon reflow in an inert atmosphere.
However, in any application, the post-assembly environment has to be taken
into consideration.  In Barbīs application, OSP was considered but the
product has to survive in potentially humid environments and thus the long
term impact on reliability has to be taken into consideration.
There is still no panacea surface finish for the industry - at least not
yet.  Everything is application specific.

Phil Zarrow
ITM Consulting
Durham, NH  USA
www.ITMconsulting.org

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2